Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler
Thermal Power Generation   Vol. 45, Issue 7, Pages: 104-109(2016)
更新时间:2025-09-28
    • Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler

    • CLC: TK223.31
    • Published:2016

    移动端阅览

  • ZHOU Ke, SHE Yuanyuan, LU Fen, et al. Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler[J]. Thermal Power Generation, 2016, 45(7): 104-109. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

263

下载量

12

CSCD

Alert me when the article has been cited
提交
Outline
No Sections

Related Articles

High temperature corrosion in wall-firing boiler:reason analysis and treatment
Influencing factors of reducing gas in water wall area of a 600 MW unit boiler
Research on influence of water wall adhering wind dip angle on high temperature corrosion in tangentially-fired boiler burning high sulfur coal
CAUSE ANALYSIS OF WATER-WALL TUBE BURST AND LEAKAGE FOR A 2100t/h BOILER
CAUSE ANALYSIS OF HIGH TEMPERATURE CORROSION OCCURRED ON THE WATER-WALL AND RESOLUTION MEASURES THEREOF

Related Author

LIU Honggang
ZHANG Guangcai
WANG Zhigang
LIAO Xiaochun
CHEN Minsheng
CHEN Yiyang
XUE Xiaolei
YU Shengjie

Related Institution

Guangdong Yuedian Jinghai Power Generation Co., Ltd
Xi'an Thermal Power Research Institute Co., Ltd. Suzhou Branch
School of Mechanical and Automotive Engineering, Shanghai University of Engineering and Technology
Inner Mongolia Special Equipment Inspection and Research Institute
Shajiao C Power Plant
0