JIN Xin1, DUAN Bao-lin1, WEI Tong-sheng2, et al. ANALYSIS OF CAUSES RESULTING IN SERIOUS SLAGGING ON SIDE-WALLS OF FW TYPE W-SHAPED FLAME BOILER[J]. Thermal Power Generation2007, (2): 37-38.
DOI:
JIN Xin1, DUAN Bao-lin1, WEI Tong-sheng2, et al. ANALYSIS OF CAUSES RESULTING IN SERIOUS SLAGGING ON SIDE-WALLS OF FW TYPE W-SHAPED FLAME BOILER[J]. Thermal Power Generation2007, (2): 37-38. DOI: 10.19666/j.rlfd.2007.02.011.
ANALYSIS OF CAUSES RESULTING IN SERIOUS SLAGGING ON SIDE-WALLS OF FW TYPE W-SHAPED FLAME BOILER
摘要
通过对某电厂FW型W火焰锅炉近壁面区域烟气温度场和流场测试
认为侧墙和翼墙卫燃带严重结渣为烟气流的冲刷所致。据此
提出了适当关小最靠侧边下挡板的开度
减弱二次风的引射作用
有效降低侧墙和翼墙的贴壁烟气流动的运行措施。实际运行结果表明
这两个部位的结渣有所减缓
效果较为明显。
Abstract
Through test of the temperature field and the flow field for flue gas in the region nearby the surface of side-walls in a FW type W-shaped flame boiler of one power plant
it is believed that the causes resulting in serious slagging on the ignition belt of side-walls was due to scouring effect of the flue gas.Based on this
operational measures for alleviating the slagging tendency on side-walls have been put forward.